The bearings are multi-metallic, consisting of tin, copper, lead, and some other alloys, so unless you want to unbond them, don't super-freeze 'em.
Rods, as long as they're not billet or forged, are perfect candidates for cryo treating. Transmission gears are also perfect candidates.